Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , Polymer , Thermoplastic , Fluoropolymer
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporative loss; and good viscosity indices.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Viscosity Measurement 117
117
Viscosity Index; ASTM D2270
Kinematic Viscosity 470 cSt

@Temperature 20.0 °C
470 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 147 cSt
147 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
ASTM D445
Molecular Weight 4100 g/mol
4100 g/mol
Evaporation Loss 0.70 %
0.70 %
22 hrs. at 149°C; ASTM 2595
1.7 %
1.7 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 22 dynes/cm
22 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 122 kg
269 lb (mass)
Mean Hertz Load; IP 239
251 kg
553 lb (mass)
Init. Seiz. Load; IP 239
447 kg
986 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.810 mm
0.0319 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 150