Polymer Property : Four Ball Extreme Pressure, Weld Load = 764.3 lb (mass) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 346.6 kg
764.3 lb (mass)
Dow Corning MOLYKOTE® 1292 LONG LIFE BEARING GREASE
For high-temperature use and applications that come in contact with solvents, fuels and water; recommended for rolling element and plain bearings. Light consistency; resists solvents, fuels and moi..
Four Ball Extreme Pressure, Weld Load 346.6 kg
764.3 lb (mass)
Dow Corning MOLYKOTE® LONGTERM 00 GREASE
NLGI 00 mineral oil greaseInformation provided by Dow Corning