Dow Corning MOLYKOTE® LONGTERM 00 GREASE

Category Fluid , Lubricant
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MOLYKOTE® LONGTERM 00 GREASE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NLGI 00 mineral oil greaseInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc

@Temperature 25.0 °C
0.930 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 300 cSt
300 cSt
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 346.6 kg
764.3 lb (mass)
Penetration P(60), 1/10 mm 400 - 430
400 - 430
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 190 °C
374 °F
Descriptive Properties Value Comments
Color black
NLGI Number 0