Mechanical Properties Metric English Comments
Four Ball Wear 0.260 mm
0.0102 in
20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
ExxonMobil 150 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Four Ball Wear 0.260 mm
0.0102 in
20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
ExxonMobil 150 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Four Ball Wear 0.260 mm
0.0102 in
Scar Diameter
ChevronTexaco StarFak® PM
Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water ..
Four Ball Wear 0.260 mm
0.0102 in
ChevronTexaco Ulti-Plex® Synthetic Grease EP
FeaturesChevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low ..