Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.260 mm | 0.0102 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Four Ball Wear | 0.260 mm | 0.0102 in | 20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172 |
ExxonMobil 150 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Four Ball Wear | 0.260 mm | 0.0102 in | Scar Diameter |
ChevronTexaco StarFak® PM Texaco Starfak PM delivers value through:Continuous high temperature stabilityLow temperature pumpabilityLow temperature lubricationExcellent oxidation, corrosion and wear protectionExcellent water .. |
|||
Four Ball Wear | 0.260 mm | 0.0102 in | |
ChevronTexaco Ulti-Plex® Synthetic Grease EP FeaturesChevron Ulti-Plex Synthetic Grease EP is a multipurpose, high performance grease specially formulated for extreme pressure bearing applications operating under the most extreme high and low .. |