Polymer Property : Four Ball Wear = 0.0217 in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.550 mm
0.0217 in
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels
Description: Elm SoyGrease™ Semi-Truck Fifth Wheel is formulated with the bestoptimized Biotechbased™ USA-grown natural seed oil that surpasses the lubricity of most conventional oils. This bi..
Four Ball Wear 0.550 mm
0.0217 in
ELM® TempFlex™ 35 to 160 Biodegradable Rail Curve Lubricant
Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed..
Four Ball Wear 0.550 mm
0.0217 in
ConocoPhillips 100 FR Hydraulic Fluid ISO
Description: Conoco FR Hydraulic Fluid is a fire-resistant, water-in-oil, invert-emulsion fluid for hydraulic systems, such as those found in underground mining equipment in which fire hazard and pe..
Four Ball Wear 0.550 mm
0.0217 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..
Four Ball Wear 0.550 mm
0.0217 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..