Material Notes:
Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed for wayside applicators with wide temperature requirementsPumps and carries when using wayside application equipment and grease temperature is between 35°F and 160°FRecommended for heavy load applications such as coal trainsRecommended for environmentally sensitive areas near waterwaysBenefits: Contains advanced extreme pressure additives and graphite for excellent protection against wheel and rail wearReduces friction and wear between track and wheel flangeFormulated to resist port plugging in wiping barsLonger carry down track from lubricatorBetter gauge face coefficient of friction than most petroleum-based greaseLess migration to top of rail than major petroleum-based greaseImproves fuel efficiency and superior lubricityHigher flash point than petroleum greases for increased safetyBiodegradable formula reduces damage to the environmentMeets EPA’s Environmental Preferable Purchasing (EPP) criteriaMeets USDA’s proposed Biobased product definition for EO 13101Manufactured from renewable USA-grown crop-based oilsInformation provided by ELM®
Physical Properties Metric English Comments
Viscosity Measurement 201
201
Base Oil, Index
Kinematic Viscosity at 40°C (104°F) 86 cSt
86 cSt
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
Four Ball Wear 0.550 mm
0.0217 in
Penetration 310
310
Cone, unworked
Thermal Properties Metric English Comments
Flash Point 326 °C
619 °F
Base Oil
Dropping Point 199 °C
390 °F
Descriptive Properties Value Comments
Appearance Dark Green to Black