Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.270 mm | 0.0106 in | Scar Diameter, 1800 rpm, 20 kg; ASTM D4172 |
ChevronTexaco Cetus® PAO 100 Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie.. |
|||
Four Ball Wear | 0.270 mm | 0.0106 in | Scar Diameter, 1800 rpm, 20 kg; ASTM D4172 |
ChevronTexaco Cetus® PAO 68 Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie.. |