ChevronTexaco Cetus® PAO 68

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ChevronTexaco Corp
Trade Name Cetus® PAO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Cetus® PAO 68.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficiency — Oxidative stability and low carbon-forming tendencies minimize sludge and deposit formation.Extended drain intervals — Long lubricant life means less frequent oil changes.Reduced maintenance and downtime — Trouble free operation and extended service intervals means reduced operating costs.Reduced oil consumption — Low volatility means less oil goes downstream, and less oil is needed for makeup.Recommended in Atlas Copco, Sullair, Ingersoll-Rand and Quincy rotary screw air compressors. Texaco Cetus PAO products meet the requirements of German DIN 51506 VDL standard.Texaco Cetus PAO oils are synthetic compressor oils. They are based on polyalphaolefin technology.They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and excellent hydrolytic stability.Texaco Cetus PAO oils protect against rust, oxidation, and foaming, and have good antiwear properties.The natural thermal and oxidation stability of these lubricants, due to their high level of purity and refinement, has been further enhanced by their unique additive systems.The high thermal and oxidation stability reduces the formation of oxidation byproducts and acidic materials which will eventually cause deposits and varnish.They are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.They minimize entrained air, which could otherwise result in reduced lubricant film thickness and potentially lead to pump cavitation.They are compatible with most elastomeric seal materials that are used with mineral oil based compressor lubricants.Texaco Cetus PAO oils are formulated to provide outstanding lubricating qualities for air compressors, especially portable and stationary rotary, vane, and screw compressors.Texaco Cetus PAO oils are recommended for industrial bearings and gears that require a synthetic gear oil that does not contain extreme pressure additives.Texaco Cetus PAO oils are designed for applications with wide operating temperature ranges. They are especially effective in high temperature applications where outstanding thermal and oxidative stability are required.Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.Do not use in breathing air apparatus or medical equipment.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222023; MSDS Number: 8903
Physical Properties Metric English Comments
API Gravity 36.5 °
36.5 °
ASTM D287
Viscosity Measurement 139
139
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 330 SUS
330 SUS
ASTM D445
Saybolt Viscosity at 210°F 60 SUS
60 SUS
ASTM D445
Kinematic Viscosity at 40°C (104°F) 64.6 cSt
64.6 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 10 cSt
10 cSt
ASTM D445
Oxidative Stability 25 hour
25 hour
to 25 psi drop; ASTM D2272
ASTM Color 0.50
0.50
L; ASTM D1500
Mechanical Properties Metric English Comments
Four Ball Wear 0.270 mm
0.0106 in
Scar Diameter, 1800 rpm, 20 kg; ASTM D4172
Thermal Properties Metric English Comments
Pour Point >= -56.0 °C
>= -68.8 °F
ASTM D97
Flash Point 262 °C
504 °F
ASTM D92
Descriptive Properties Value Comments
Corrosion, Copper Strip 1a
3 h at 100°C
Foaming Stability, mL 0
ASTM D892, Sequence II
Foaming Tendency, mL 20
ASTM D892, Sequence II
Noack Volatility, wt% 3
DIN 51581
Rust Prevention Pass
Synthetic sea water
Water Separability min 10
to 0 ml emulsion