Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Four Ball Wear = 0.370 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.370 mm
0.0146 in
Scar Diameter
ConocoPhillips EP Conolith® HT Grease NLGI NO. 1
Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh..
Four Ball Wear 0.370 mm
0.0146 in
Scar Diameter
ConocoPhillips EP Conolith® HT Grease NLGI NO.2
Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh..