Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ConocoPhillips EP Conolith® HT Grease NLGI NO.2

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips EP Conolith® HT Grease NLGI NO.2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wheel bearings in automotive and commercial service. It is recommended for industrial applications, such as heavily loaded antifriction and plain bearings commonly found in industry where an EP, water-resistant, high-temperature grease is required. EP Conolith HT Grease is certified for use in automotive and commercial vehicles and carries NLGI GC-LB approval. At high temperatures, EP Conolith HT Grease continues to lubricate and resists melting up to 400°F (200°C), which prevents leakage from the bearing seals and subsequent bearing failure.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 70
70
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 732 SUS
732 SUS
Base Oil Property
Saybolt Viscosity at 210°F 68 SUS
68 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 158 cSt
158 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 12.5 cSt
12.5 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Load
Four Ball Wear 0.370 mm
0.0146 in
Scar Diameter
Penetration P(60), 1/10 mm 280
280
Timken Test 24900 g
55.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Dropping Point 260 °C
500 °F
Descriptive Properties Value Comments
ASTM Rust A&B Pass
Color Amber
Low Temperature Mobility 0.1 gm/sec
at 0°F
0.3 gm/sec
at 10°F
0.5 gm/sec
at 20°F
Oil Separation 0.5 wt.%
Shear Stability +5% in Consistency
Roll Stability
Soap Type (Thickener) Lithium Complex
Water Washout 11%
at 175°F
5%
at 100°F
Wheel Bearing Leakage 1 wt.%
at 212°F
13 wt.%
at 325°F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved