Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.410 mm | 0.0161 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Mobil Polyrex EM Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | 1800 rpm |
ChevronTexaco HiPerSYN™ ISO 32 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | 1800 rpm |
ChevronTexaco HiPerSYN™ ISO 46 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | 1800 rpm |
ChevronTexaco HiPerSYN™ ISO 68 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | |
ChevronTexaco Wheel End Grease FeaturesChevron Wheel End Grease is a high performance grease specifically engineered for trailer wheel-ends operating in most conditions.It is formulated with ISOSYN™ base stocks, a unique polyure.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | 40 kg, 1200 rpm, 75°C, 1 hr; ASTM D2266 |
ExxonMobil Mobil Polyrex EM Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | |
ConocoPhillips EP Conolith® Grease NLGI NO. 0 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Four Ball Wear | 0.410 mm | 0.0161 in | |
ConocoPhillips EP Conolith® Grease NLGI NO. 000 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |