Material Notes:
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for these bearings when they are subjected to high speeds, moderate temperatures, water and shock loads. It does not contain any tackifiers, which makes it ideal for centralized lubrication systems. EP Conolith Grease is available in several NLGI grades and has been widely accepted in the steel, aluminum and other industries as a general-purpose plant grease. EP Conolith Grease is widely used by the can manufacturing industry because it has, in addition to the required performance characteristics, a light, low-staining, natural color. EP Conolith Grease is manufactured with high-viscosity index paraffinic basestocks and lithium 12-Hydroxy stearate soap stock. It is compounded with an effective extreme-pressure additive and corrosion inhibitors which impart good load-carrying characteristics and good chemical stability.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 95
95
Viscosity Index
Saybolt Viscosity at 100°F 880 SUS
880 SUS
Base Oil Property
Saybolt Viscosity at 210°F 86 SUS
86 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
Four Ball Wear 0.410 mm
0.0161 in
Penetration P(60), 1/10 mm 460
460
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -20.6 °C
-5.00 °F
Pour Point -12.2 °C
10.0 °F
Dropping Point 163 °C
325 °F
Descriptive Properties Value Comments
ASTM Rust A&B Pass
Color Green/Brown
Low Temperature Mobility 0.5 gm/sec
at 0°F
1 gm/sec
at 10°F
2.1 gm/sec
at 20°F
Shear Stability +5% in Consistency
Roll Stability
Soap Type (Thickener) Lithium
Water Washout 11%
at 100°F
39%
at 175°F