Polymer Property : Izod Impact, Notched (ISO) = 0.904 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.90 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
0.904 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Polimeri Europa Edistir N 2380 Polystyrene
High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla..
Izod Impact, Notched (ISO) 1.90 kJ/m²

@Temperature -40.0 °C
0.904 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer
Description: Hostacom™ ZB752AC precolored, medium melt flow, 2,800 MPa flexural modulus, mineral-filled polypropylene homopolymer has a very good combination of strength, stiffness, and impact resi..