Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.90 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
0.904 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir N 2380 Polystyrene High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla.. |
|||
Izod Impact, Notched (ISO) | 1.90 kJ/m² @Temperature -40.0 °C |
0.904 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer Description: Hostacom™ ZB752AC precolored, medium melt flow, 2,800 MPa flexural modulus, mineral-filled polypropylene homopolymer has a very good combination of strength, stiffness, and impact resi.. |