Polymer Property : Izod Impact, Notched (ISO) = 17.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, Conditioned
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 49 Nylon 66, Conditioned
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DSM Arnitel® PM650 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DSM Arnitel® PM650 Polyether Ester Elastomer (European and Asian Grade)