Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 2.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Eastar GN002 Copolyester, Natural  (discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Eastar GN005 Copolyester, Natural  (discontinued **)
Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -17.8 °C
2.00 ft-lb/in²

@Temperature 0.000 °F
ISO 180/1A
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol..
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180
LyondellBasell Hifax™ HSBMCB1158LS Thermoplastic Polyolefin Elastomer
Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impa..