Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hifaxâ„¢ RTA3263/2 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impac..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® E309 ABS
Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber
SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade
SAXAMID 136Q32 is a high impact-modified polyamide 6 injection-molding-grade.Information provided by SAX Polymers
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -40.0 °C
9.99 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl LS175 PPE+HIPS
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 22.0 °C
9.99 ft-lb/in²

@Temperature 71.6 °F
ISO 180
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers
Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DSM Arnitel® PL650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -40.0 °C
9.99 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -20.0 °C
9.99 ft-lb/in²

@Temperature -4.00 °F
Edgew 80x10x4; ISO 180/1A
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66  (Unverified Data**)
Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber