Polymer Property : Izod Impact, Notched (ISO) = 46.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 46.0 kJ/m²

@Temperature 0.000 °C
21.9 ft-lb/in²

@Temperature 32.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East)
High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..
Izod Impact, Notched (ISO) 46.0 kJ/m²

@Temperature 0.000 °C
21.9 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Izod Impact, Notched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer
Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint..
Izod Impact, Notched (ISO) 46.0 kJ/m²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Dow INSPIRE™ 112 Performance Polymer
INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow