Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Thickness 4.00 mm, Temperature -30.0 °C |
2.86 ft-lb/in² @Thickness 0.157 in, Temperature -22.0 °F |
ISO 180/1A |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1000V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in .. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East) GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East) Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used .. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD1607 PBT+PC (Europe-Africa-Middle East) 22% Glass filled PBT+PC with a designed balance between surface appearance and mechanical properties sufficient for automotive doorhandle requirements. Special suitable for gas assist mouldings .Thi.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -40.0 °C |
2.86 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 NL TD20 PBT, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR15 NL PA 6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 KG30 NL 0G PA6, 30% glass fiber/glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat.. |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.Information .. |