Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
4.04 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Polimeri Europa Edistir ICE S 800/N Polystyrene  (discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -20.0 °C
4.04 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced
GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -20.0 °C
4.04 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced
GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -30.0 °C
4.04 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Polyram RamSter PF305G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -20.0 °C
4.04 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified
Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
Izod Impact, Notched (ISO) 8.50 kJ/m²

@Temperature -40.0 °C
4.04 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..