Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 9.50 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
4.52 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin
Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req..
Izod Impact, Notched (ISO) 9.50 kJ/m²

@Temperature -30.0 °C
4.52 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
Izod Impact, Notched (ISO) 9.50 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
4.52 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Polimeri Europa Sinkral® D 232/M3 ABS Resin  (discontinued **)
Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr..
Izod Impact, Notched (ISO) 9.50 kJ/m²

@Temperature 23.0 °C
4.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..