Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.60 kJ/m² @Temperature -30.0 °C |
4.57 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 180/1A |
EMS-Grivory Grivory® R 47 HW 10 PA6 Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion .. |