Material Notes:
Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion lines, as well as on rod and profile extrusion equipment. Grilon R 47 HW 10 was specially developed for the production of small diameter mandrels which are used for the manufacturing of rubber hoses.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 10 %
10 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
dry; ISO 527-1/-2
46.0 MPa
6670 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 34.0 MPa
4930 psi
dry; ISO 527-1/-2
34.0 MPa
4930 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 16 %
16 %
dry; ISO 527-1/-2
16 %
16 %
dry; ISO 527-1/-2
Tensile Modulus 0.430 GPa
62.4 ksi
conditioned; ISO 527-1/-2
0.940 GPa
136 ksi
dry; ISO 527-1/-2
Izod Impact, Notched (ISO) 7.50 kJ/m²

@Temperature -30.0 °C
3.57 ft-lb/in²

@Temperature -22.0 °F
conditioned; ISO 180/1A
9.60 kJ/m²

@Temperature -30.0 °C
4.57 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 180/1A
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
conditioned; ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
ISO 75-1/-2
Vicat Softening Point 159 °C
318 °F
50°C/h 50N; ISO 306
210 °C
410 °F
ISO 306
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Compressed air systems
Cooling and climate control
Fuel systems
Hydraulic systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Masterbatch
Special Characteristics Improved heat resistance
Copyright © lookpolymers.com All Rights Reserved