Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 104 MPa @Temperature 23.0 °C |
15100 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |