Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 840 - 1000 MPa @Thickness 65.0 mm |
122000 - 145000 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Tensile Strength at Break | 840 - 1000 MPa @Thickness 65.0 mm |
122000 - 145000 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |