Tensile Strength at Break 12.0 MPa

@Temperature 23.0 °C
1740 psi

@Temperature 73.4 °F
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N..
Tensile Strength at Break 12.0 MPa

@Temperature 90.0 °C
1740 psi

@Temperature 194 °F
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..