Polymer Property : Tensile Strength at Break = 175 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa

@Temperature 125 °C
25400 psi

@Temperature 257 °F
ISO 527
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 175 MPa

@Temperature 90.0 °C
25400 psi

@Temperature 194 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Strength at Break 175 MPa

@Temperature 90.0 °C
25400 psi

@Temperature 194 °F
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Tensile Strength at Break 175 MPa

@Temperature 60.0 °C
25400 psi

@Temperature 140 °F
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
Dry; EN2561
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Strength at Break 175 MPa

@Temperature 23.0 °C
25400 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..