Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 190 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 190 MPa

@Temperature 300 °C
>= 27600 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 190 MPa

@Temperature 125 °C
27600 psi

@Temperature 257 °F
ISO 527
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Tensile Strength at Break 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 190 MPa

@Temperature 150 °C
27600 psi

@Temperature 302 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &..
Tensile Strength at Break 190 MPa

@Temperature 120 °C
27600 psi

@Temperature 248 °F
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; ..
Tensile Strength at Break 190 MPa

@Temperature 60.0 °C
27600 psi

@Temperature 140 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Strength at Break 190 MPa

@Temperature 90.0 °C
27600 psi

@Temperature 194 °F
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Strength at Break 190 MPa

@Temperature 1093 °C
27600 psi

@Temperature 1999 °F
Plate; Transverse
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL..
Tensile Strength at Break 190 MPa

@Temperature -10.0 °C
27600 psi

@Temperature 14.0 °F
ASTM D638
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Tensile Strength at Break 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..