Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 156 MPa @Temperature -40.0 °C |
22600 psi @Temperature -40.0 °F |
ISO 527-1/-2 |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |