Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 161 MPa @Temperature 250 °C |
>= 23400 psi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |