Polymer Property : Tensile Strength at Break = 2740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.9 MPa

@Temperature 100 °C,
Time 259000 sec
2740 psi

@Temperature 212 °F,
Time 72.0 hour
Circulating Oven Aging
LG Chemical NBR 6240 High Acrylonitrile Polymer
Description: NBR 6240 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6240 is a non staining, medium low mooney..