Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 65.5 MPa @Temperature 100 °C |
9500 psi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Tensile Strength at Break | 65.5 MPa @Temperature 100 °C |
9500 psi @Temperature 212 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |