Mechanical Properties Metric English Comments
Tensile Strength at Break 65.5 MPa

@Temperature 100 °C
9500 psi

@Temperature 212 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Strength at Break 65.5 MPa

@Temperature 100 °C
9500 psi

@Temperature 212 °F
2; ISO 527-2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..