Mechanical Properties Metric English Comments
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
Cadi 1 MOLD-MOR™
A very hard heat treatable copper alloy with moderate electrical conductivity. C18000 offers excellent value for the properties it offers. C18000 is a viable substitute for C17500 and C17510 for m..
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
Cadi 10 MOLD-MOR™
A Copper Nickel Silicon Chromium Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company.
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
Cadi 2 MOLD-MOR™
A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an..
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
Cadi 20 MOLD-MOR™
A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company.
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
Cadi C17500 Copper Alloy
Information provided by Cadi Company.