Material Notes:
A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical and thermal electrical conductivity are required.Forms: RodBarPlateInformation provided by Cadi Company.
Physical Properties Metric English Comments
Density 8.77 g/cc
0.317 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B >= 90
>= 90
Any thickness
Tensile Strength at Break >= 607 MPa

@Thickness >=50.8 mm
>= 88000 psi

@Thickness >=2.00 in
>= 621 MPa

@Thickness 25.4 - 50.8 mm
>= 90000 psi

@Thickness 1.00 - 2.00 in
>= 648 MPa

@Thickness <=25.4 mm
>= 94000 psi

@Thickness <=1.00 in
Tensile Strength, Yield >= 607 MPa

@Strain 0.500 %,
Thickness >=50.8 mm
>= 88000 psi

@Strain 0.500 %,
Thickness >=2.00 in
>= 621 MPa

@Strain 0.500 %,
Thickness 25.4 - 50.8 mm
>= 90000 psi

@Strain 0.500 %,
Thickness 1.00 - 2.00 in
>= 648 MPa

@Strain 0.500 %,
Thickness <=25.4 mm
>= 94000 psi

@Strain 0.500 %,
Thickness <=1.00 in
Modulus of Elasticity 131 GPa
19000 ksi
Poissons Ratio 0.267
0.267
Shear Modulus 51.7 GPa
7500 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 225 W/m-K
1560 BTU-in/hr-ft²-°F
Melting Point 1029 - 1068 °C
1885 - 1955 °F
Solidus 1029 °C
1885 °F
Liquidus 1068 °C
1955 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.40 %
0.40 %
Copper, Cu 97.8 %
97.8 %
Nickel, Ni 1.8 %
1.8 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000383 ohm-cm
<= 0.00000383 ohm-cm
Calculated from Min 45 %IACS, up to 3" diameter/any thickness
Processing Properties Metric English Comments
Processing Temperature 788 °C
1450 °F
Brazing
Descriptive Properties Value Comments
RMWA Class 3