Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1090 MPa | 158000 psi | ASTM-D790 |
Braskem GM5010T2 HDPE High Density Extrusion Polyethylene GM5010T2 is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes. It is produced with bimodal technology and has high molar mass. It shows high mechanical.. |
|||
Flexural Modulus, 1% Secant | 1090 MPa | 158000 psi | ASTM-D790 |
Braskem GM5010T2B HDPE High Density Extrusion Polyethylene GM5010T2B is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. .. |