Polymer Property : Flexural Modulus, 1% Secant = 158000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1090 MPa
158000 psi
ASTM-D790
Braskem GM5010T2 HDPE High Density Extrusion Polyethylene
GM5010T2 is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes. It is produced with bimodal technology and has high molar mass. It shows high mechanical..
Flexural Modulus, 1% Secant 1090 MPa
158000 psi
ASTM-D790
Braskem GM5010T2B HDPE High Density Extrusion Polyethylene
GM5010T2B is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. ..