Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM D790A |
SABIC PP 651H Polypropylene Random Copolymer for PIPE Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App.. |
|||
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM-D790 |
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive.. |
|||
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM-D790 |
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. .. |
|||
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM-D790 |
Braskem PRB 0131 RACO Random Polypropylene Copolymer PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h.. |
|||
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM-D790 |
Braskem Prisma 2400 RACO Random Polypropylene Copolymer Prisma 2400 is a high melt flow rate random copolymer. This product is designed for the ISBM (Injection Stretch Blow Molding) process and offers low taste/odor. It can also be used in the blow moldi.. |
|||
Flexural Modulus, 1% Secant | 900 MPa | 131000 psi | ASTM D790A |
Braskem CP 741 Extrusion Polypropylene Heterophasic Copolymer Sheet extrusion.Information provided by Braskem. |