Polymer Property : Flexural Modulus, 1% Secant = 164000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1130 MPa
164000 psi
ASTM D790
Flint Hills 23H2A Random Copolymer Polypropylene
Features: Excellent clarity. Product does not contain animal derived components.Applications: Designed for Blow molding and Thermoforming - A replacement for PET, PS and PC high clarity applicatio..