Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1430 MPa @Temperature 23.0 °C |
207000 psi @Temperature 73.4 °F |
0.05 in/min test speed |
Ineos H04G-00 Polypropylene Homopolymer This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications... |