Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 580 MPa | 84100 psi | ASTM D 790 |
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |