Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 965 MPa @Temperature 23.0 °C |
140000 psi @Temperature 73.4 °F |
0.05 in/min test speed |
Ineos N20N-00 Polypropylene Impact Copolymer This is a high melt flow rate, nucleated polypropylene impact copolymer formulated for improved flowability. It has an optimum balance of stiffness and impact resistance for injection molded applic.. |
|||
Flexural Modulus, 1% Secant | 965 MPa | 140000 psi | ASTM D790 |
ExxonMobil HDPE HD 7800P High Density Polyethylene Copolymer Resin Product Description: HD 7800P is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds.. |
|||
Flexural Modulus, 1% Secant | 965 MPa | 140000 psi | ASTM D-790A |
Bapolene® 5065NB Polypropylene Impact Copolymer Description: Impact copolymer for injection molding applications. It is nucleated and exhibits superior low temperature resistance.Applications: Injection molding and compounding.Information provid.. |