Mechanical Properties Metric English Comments
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:4
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..