Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Stainless Steel Fiber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.41 - 1.79 g/cc
0.0509 - 0.0647 lb/in³
Average value: 1.61 g/cc Grade Count:10
Water Absorption 0.0200 - 0.600 %
0.0200 - 0.600 %
Average value: 0.407 % Grade Count:3
Linear Mold Shrinkage 0.00200 - 0.0160 cm/cm
0.00200 - 0.0160 in/in
Average value: 0.00520 cm/cm Grade Count:7
Linear Mold Shrinkage, Transverse 0.0100 cm/cm
0.0100 in/in
Average value: 0.0100 cm/cm Grade Count:3
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.0 - 117 MPa
6820 - 17000 psi
Average value: 83.8 MPa Grade Count:8
Elongation at Break 0.500 - 2.00 %
0.500 - 2.00 %
Average value: 1.43 % Grade Count:8
Modulus of Elasticity 3.79 - 12.4 GPa
550 - 1800 ksi
Average value: 7.63 GPa Grade Count:8
Flexural Yield Strength 103 - 207 MPa
15000 - 30000 psi
Average value: 153 MPa Grade Count:10
Flexural Modulus 4.00 - 13.8 GPa
580 - 2000 ksi
Average value: 9.50 GPa Grade Count:10
Izod Impact, Notched 0.267 - 0.801 J/cm
0.500 - 1.50 ft-lb/in
Average value: 0.493 J/cm Grade Count:9
Izod Impact, Unnotched 1.60 - 3.20 J/cm
3.00 - 5.99 ft-lb/in
Average value: 2.25 J/cm Grade Count:7
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
Average value: 10100 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 254 - 260 °C
489 - 500 °F
Average value: 257 °C Grade Count:6
Flammability, UL94 V-0
V-0
Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 1.00e+7 ohm-cm
1.00 - 1.00e+7 ohm-cm
Average value: 1.11e+6 ohm-cm Grade Count:9
Surface Resistance 100 - 1.00e+7 ohm
100 - 1.00e+7 ohm
Average value: 1.84e+6 ohm Grade Count:6
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.00 sec Grade Count:3
Processing Properties Metric English Comments
Melt Temperature 300 - 329 °C
572 - 625 °F
Average value: 313 °C Grade Count:4
Mold Temperature 135 - 177 °C
275 - 350 °F
Average value: 156 °C Grade Count:4
Drying Temperature 149 - 270 °C
300 - 518 °F
Average value: 178 °C Grade Count:4
Moisture Content 0.0400 - 0.200 %
0.0400 - 0.200 %
Average value: 0.0800 % Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:4