K (wear) Factor 328 x 10-8 mm³/N-M
163 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..