Polymer Property : K (wear) Factor = 3.50 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 3.50 x 10-8 mm³/N-M
1.74 x 10-10 in³-min/ft-lb-hr
LATI Latilub 87/24UV-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). UV stabilized. PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
K (wear) Factor 3.50 x 10-8 mm³/N-M
1.74 x 10-10 in³-min/ft-lb-hr
LATI Latilub 87/28-20T PC, PTFE Filled
Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A.
K (wear) Factor 3.50 - 100 x 10-8 mm³/N-M
1.74 - 49.6 x 10-10 in³-min/ft-lb-hr
Average value: 53.8 x 10<sup>-8</sup> mm³/N-M Grade Count:6
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..