Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 8.00 - 94.7 x 10-8 mm³/N-M | 3.97 - 47.0 x 10-10 in³-min/ft-lb-hr | Average value: 36.0 x 10<sup>-8</sup> mm³/N-M Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
K (wear) Factor | 8.00 x 10-8 mm³/N-M | 3.97 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
K (wear) Factor | 8.00 x 10-8 mm³/N-M | 3.97 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 80-10T K/15 PPS, 15% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |