K (wear) Factor 8.00 - 94.7 x 10-8 mm³/N-M
3.97 - 47.0 x 10-10 in³-min/ft-lb-hr
Average value: 36.0 x 10<sup>-8</sup> mm³/N-M Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..