Mechanical Properties Metric English Comments
K (wear) Factor 4.43 x 10-8 mm³/N-M
2.20 x 10-10 in³-min/ft-lb-hr
Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..